| Product Name | DENKA DCR-40 |
| Chemical Type | Chloroprene Rubber (CR) |
| Appearance | Pale Amber Chips |
| Mooney Viscosity Ml 1plus4 100c | 40 |
| Crystallization Rate | Rapid |
| Specific Gravity | 1.23 |
| Volatile Matter Content | 0.4% max |
| Ash Content | 0.7% max |
| Tensile Strength | 24 MPa |
| Elongation At Break | 800% |
| Oil Resistance | Good |
| Ozone Resistance | Excellent |
| Self Reinforcing | Yes |
As an accredited DENKA DCR-40 Chloroprene Rubber (CR) factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | The DENKA DCR-40 Chloroprene Rubber (CR) is packaged in 25 kg paper bags with an inner polyethylene liner for moisture protection. |
| Storage | DENKA DCR-40 Chloroprene Rubber (CR) should be stored in a cool, dry, and well-ventilated area, away from direct sunlight, heat sources, and moisture. Keep the material in its original, tightly sealed packaging to prevent contamination. Avoid exposure to strong acids, alkalis, and oxidizing agents. Proper storage conditions help maintain the product’s quality and extend its shelf life. |
| Shipping | DENKA DCR-40 Chloroprene Rubber (CR) is typically shipped in securely sealed, multi-layer kraft paper bags or cartons, each containing 25 kg. The material should be stored and transported in a cool, dry place, away from direct sunlight and sources of heat to maintain its quality and prevent degradation. |
Competitive DENKA DCR-40 Chloroprene Rubber (CR) prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com