506885 |
| Appearance | Gray paste |
| Base Polymer | Silicone |
| Curing System | Addition cure (platinum-catalyzed) |
| Hardness | Shore A 60 |
| Tensile Strength | 3.4 MPa |
| Elongation | 160% |
| Tear Strength | 8 kN/m |
| Specific Gravity | 1.30 |
| Operating Temperature Range | -40°C to +200°C |
| Cure Time | 24 hours at room temperature |
| Skin Over Time | 10 minutes |
| Volume Resistivity | 1.0 x 10^15 Ω·cm |
As an accredited Shin-Etsu KE-961T-U Silicone Rubber factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Shin-Etsu KE-961T-U Silicone Rubber is packaged in a 1 kg white metal can with distinctive blue labeling and product details. |
| Storage | Shin-Etsu KE-961T-U Silicone Rubber should be stored in a cool, dry place, away from direct sunlight and sources of heat. Keep the container tightly sealed to prevent contamination and moisture absorption. Recommended storage temperature is below 25°C (77°F). Proper storage ensures maximum shelf life and maintains material quality for optimal performance during processing and application. |
| Shipping | Shin-Etsu KE-961T-U Silicone Rubber should be shipped in sealed, labeled containers, protected from moisture and direct sunlight. Store and transport at temperatures below 30°C. Ensure compliance with local regulations; the product is generally non-hazardous, but avoid exposure to extreme temperatures during transit to maintain material integrity and quality. |
Competitive Shin-Etsu KE-961T-U Silicone Rubber prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8615365186327 or mail to sales3@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8615365186327
Email: sales3@ascent-chem.com